What is really going on under the floor

A fiberglass tub or shower base is a fairly thin shell. On its own it is not strong enough to carry a person standing in it; it relies on solid support underneath to keep the floor from moving. When that support breaks down, or was never fully filled in when the tub was installed, the floor has nothing to rest on. Every time someone steps in, it bends a little. Fiberglass can only take so much of that before it cracks.

That is why we say all the cracks in a fiberglass tub floor come back to one thing: a lack of support under the floor. The crack you can see is the end result of movement you can feel.

How to check your own tub

  • Stand in the tub and shift your weight. If the floor moves, dips, or feels soft and spongy, the support underneath has given way.
  • Listen. Creaking or crackling sounds when you step in are a sign of the floor flexing.
  • Look at the crack pattern. Long cracks running from the front of the tub toward the back, or a spiderweb of cracks around the drain, usually point to flexing rather than a dropped object.
  • Check below the bathroom. Water stains on the ceiling under the tub mean water is already getting through.
  • Think about past repairs. If a crack was fixed and came back, that is a strong sign the support was never dealt with.

Why surface repairs fail

A filler or patch can make a crack disappear, but it cannot stop the floor from bending. If the support is not fixed, the floor keeps flexing and the crack works its way back through, often within months. We see this all the time. On a recent shower floor job in Cochrane, the floor had already been repaired once and failed. When we opened it up, there was no subfloor at all under half of the shower base, and water had been leaking onto the kitchen ceiling below. The earlier repair never had a chance.

How we fix it for good

The fix always starts with the support, not the crack. We drill small holes in the tub floor and inject a high-density foam to fill the empty space underneath, so the floor has something solid to rest on again. Then, depending on the tub and how much damage there is, we use one of three approaches:

  • Stabilize with foam only. On some tubs, the high-density foam alone is enough to stop the flexing, and no fiberglass matting is needed. We then repair the cracks and the holes we drilled, then refinish the floor.
  • Reinforce the floor. We repair the damaged area, lay fiberglass matting over the entire floor to add a full layer of strength, and refinish the floor with a new coating colour matched as closely as possible to the rest of your tub.
  • Install a tub inlay. For floors with heavier damage, a fiberglass tub inlay is fitted and bonded over the old floor, making it solid and watertight. The Cochrane shower above was an inlay installation: because half the subfloor was missing, we rebuilt the backing and plywood underneath, then two layers of heavy fiberglass matting created the new inlay over the floor.

All three are done with the tub in place: no tearing out tile, no plumbing work. If you are not sure which one your tub needs, our guide on choosing between an inlay and a repair explains the difference, and we will tell you straight after seeing it.

Do not wait on a soft floor

A flexing floor only gets worse. Cracks let water reach the subfloor and the ceiling below, which turns a one-day repair into a much bigger job, and a floor with no support underneath can eventually give way under someone's weight. If your tub or shower floor feels soft, or you can see cracks spreading, email photos to blackstonerefinishing@gmail.com or call 403 630 6534. We have been repairing fiberglass tubs across Calgary and southern Alberta since 2002.